I just switched to QTX from an Autotype product and I am having problems.

When washing out after exposing the design looks like it has no emulsion left where exposure was blocked by my film but when I try to push ink through it there are some spots that have a clear film that blocks the ink. During washout these clear blocked areas are not visible when wet and look just like the areas that have correctly washed out.

What is causing this?

How can I prevent it?

Is there a way to remove the blockage on press without damaging the rest of the screen?

 

____________________
Riley Hopkins 8/4
WorkHorse Point 1K Exposure Unit
WorkHorse Primus 18x20 Flash
WorkHorse Compact Conveyer Dryer
Dual 500 Mac G4, 1.5GB RAM, OS X 10.3.9, 1TB storage
 
View Member's Profile  View All Posts By This Member     
 
This thread:
[ Home | ScreenPrinters.net | Feedback | Register | Profile | FAQ | Help ] [ Login | Lost Password ]

Only registered members may post to the Boards.

Need to register? It's free!

Having trouble posting after logging in? Click Here