| Posted on 2/20/07 at 01:03 AM | |
|
|
From Union's site description it sounds like it needs the same cure as any other plastisol from Union which is 300 degrees all the way through the ink deposit. http://www.unionink.com/products/special/pagl-m.html [Edited on 2/20/07 by Light_Speed] ____________________ Riley Hopkins 8/4 WorkHorse Point 1K Exposure Unit WorkHorse Primus 18x20 Flash WorkHorse Compact Conveyer Dryer Dual 500 Mac G4, 1.5GB RAM, OS X 10.3.9, 1TB storage | |
|