| Posted on 4/3/08 at 02:51 AM | |
|
hi, thanks ever so much for getting back to me.. this thing is driving me mad! i'm using a super primex sp-10 (not the greatest machine in the world.. but hey!) when i make the plate I initially expose for 2 minutes, then i take off the transparency and expose with the tint for however long.. then wash. I then expose for a further 10 minutes for hardening... as per the instructions I have here. Ink... at the minute i have 2 small post of marabu ink and I'm just mixing that with 10% thinner. any help would be appreciated. Lay [Edited on 4/3/08 by lprice80] ____________________ all i want to do is simple printing!! | ||
|
Hi Frank, welcome back.... by Panker - on 4/7/08 at 08:57 AMOnly registered members may post to the Boards.