  have not ptinted foil in awhile, test prints showing a pitted look. using high density clear on a 125 mesh. curing at normal t-shirt dryer speed. foil application 8-10 seconds, 350 degrees noral pressure, peel cold. Any suggestions on which variable to start changing?  