| Posted on 5/1/08 at 05:22 AM | |
| Not sure I can analyze the problem with just the information that was presented, but here would be my guess. Being that these are dark garments I assume that you are pfp the image. I would say that if the top coat is cracking and peeling off then you have a flash cure issue. That being the flash is curing the first pass ink which will not allow the ink to re-gel through the dryer to bond with the top coat. | ||
|